Process Developed:
Machine: Mr Deburr DB300
- 1.5 Hours with ceramic ATS 7/8 X 3/8 SF
- Compound: VF100
Results:
Plastic parts are notoriously difficult o run in a tumbling process. For this part the goal was to remove the mold parting line and impart a matte finish for a second post process. We chose a fast cutting, large size ceramic media in order to effectively abrade the plastic. The tumbling process has removed the raised parting line quite effectively in a short period of time. This result is seen on all parts both glass and iron filled.
Before on Left, After On Right